Yawanci sun haɗa da: Ni-Cr alloy foda, Ni-Cr-Mo foda foda, Ni-Cr-Fe alloy foda, Ni-Cu alloy foda, Ni-P da Ni-Cr-P gami foda, Ni-Cr-Mo-Fe Alloy foda, Ni-Cr-Mo-Si high wear-resistant gami foda, Ni-Cr-Fe-Al alloy foda, Ni-Cr-Fe-Al-B-Si gami foda, Ni-Cr-Si alloy foda , Ni- Cr-W-tushen lalacewa-mai jurewa da lalata-resistant gami foda, da dai sauransu.
An samar da foda mai ɗorewa na nickel ta hanyar ƙara yawan adadin B da Si zuwa foda na nickel.Abin da ake kira kai-fluxing alloy foda, wanda kuma aka sani da eutectic alloy, mai wuyar fuska alloy, shi ne jerin foda da aka samar ta hanyar ƙara abubuwa masu haɗaka (yafi boron da silicon) wanda zai iya haifar da ƙananan narkewa a cikin nickel, cobalt, da kuma ƙarfe na tushen ƙarfe.Kayan abu.
Abubuwan da ake amfani da su na nickel da aka fi amfani da su sun haɗa da Ni-B-Si alloy foda, Ni-Cr-B-Si alloy foda, Ni-Cr-B-Si-Mo, Ni-Cr-B-Si-Mo-Cu , High-molybdenum-nickel-based self-fluxing alloy foda, high-chromium-molybdenum-nickel-based self fluxing alloy foda, Ni-Cr-WC-based self fluxing alloy foda, high jan karfe kai-fluxing gami foda, tungsten carbide watsawa nickel tushen kai-fluxing foda Alloy foda, da dai sauransu.
Matsayin abubuwan boron da silicon: yana rage mahimmancin narkewa na gami, fadada yankin zafin jiki mai ƙarfi, da samar da eutectic mai ƙarancin narkewa;rage deoxidation da slag-forming ayyuka;hardening da ƙarfafa sutura.